Use suggestion
This product can be used as a cathode material in the manufacture of lithium ion secondary batteries.
The full battery design capacity of this product with graphite negative electrode: 188 ~ 190mAh / g (0.5C, 4.2V-3.0V) (affected by the customer's process, the data has a certain degree of fluctuation)
It is recommended to bake the material at 120 ºC for 6h before mixing.
Processing design compaction 3.30 ~ 3.50g / cm3 (Affected by the customer's process, the data has a certain degree of fluctuation).
According to the performance requirements, choose an appropriate electrolyte that matches the high nickel nickel-cobalt manganese oxide.
Project | Unit | Standard | Reference | The analytical methods |
Li | % | 7.0~7.6 | 7.3 | ICP |
Ni+Co+Mn | % | 59.5±1.0 | 58.9 | ICP |
Ni | mol% | 83.0±0.7 | 82.6 | ICP |
Co | mol% | 12.0±0.5 | 12.2 | ICP |
Mn | mol% | 5.0±0.5 | 5.2 | ICP |
Ca | % | ≤0.0100 | 0.0044 | ICP |
Cu | % | ≤0.0020 | 0.0001 | ICP |
Fe | % | ≤0.0050 | 0.0005 | ICP |
Na | % | ≤0.0300 | 0.0223 | ICP |